TAILIEUCHUNG - Corrosion failure analysis of copper heat exchanger by using a non destructive technique

Temperature is directly proportional to the pH because of copper oxide layer formed as semi-protective layer to protect the metal surface from corrode and decrease the corrosion rate. With higher of temperature, the copper concentration increase. This is because of extreme environment which is in very high or very low pH will break down the protective layer and effect the concentration of water samples. As a conclusion, the NDT methods used have significantly determine the corrosion failure analyses. | Corrosion failure analysis of copper heat exchanger by using a non destructive technique

TAILIEUCHUNG - Chia sẻ tài liệu không giới hạn
Địa chỉ : 444 Hoang Hoa Tham, Hanoi, Viet Nam
Website : tailieuchung.com
Email : tailieuchung20@gmail.com
Tailieuchung.com là thư viện tài liệu trực tuyến, nơi chia sẽ trao đổi hàng triệu tài liệu như luận văn đồ án, sách, giáo trình, đề thi.
Chúng tôi không chịu trách nhiệm liên quan đến các vấn đề bản quyền nội dung tài liệu được thành viên tự nguyện đăng tải lên, nếu phát hiện thấy tài liệu xấu hoặc tài liệu có bản quyền xin hãy email cho chúng tôi.
Đã phát hiện trình chặn quảng cáo AdBlock
Trang web này phụ thuộc vào doanh thu từ số lần hiển thị quảng cáo để tồn tại. Vui lòng tắt trình chặn quảng cáo của bạn hoặc tạm dừng tính năng chặn quảng cáo cho trang web này.